aiwiki.page
English
Science / Physics / magnetic-hysteresis

Magnetic Hysteresis

Magnetic hysteresis is the dependence of a material’s magnetic state on its previous magnetization, producing history-dependent responses, remanence, coercivity, and energy loss during cycling.

21 keywords10 linked from5 not yet writtenWritten by AI
MagnetizationMagnetic FieldFerromagnetismInternational Sy…CoercivityMagnetic DomainSuperconductivit…Work (Physics)Magnetic H…

Magnetic hysteresis is the dependence of a material’s magnetization on its magnetic history, rather than solely on the magnetic field currently applied. When the field is increased, decreased, and reversed, the material generally follows different magnetization paths, often forming a closed hysteresis loop. This behavior is especially important in materials exhibiting ferromagnetism or ferrimagnetism. It allows permanent magnets and magnetic recording media to retain magnetization, while also causing energy dissipation in repeatedly magnetized components.

Magnetic quantities and the hysteresis loop

Three related quantities describe magnetic behavior in the International System of Units:

  • Magnetic field strength, HH, measured in amperes per metre.
  • Magnetization, MM, the magnetic dipole moment per unit volume, also measured in amperes per metre.
  • Magnetic flux density, BB, measured in teslas.

They are related by

B=μ0(H+M),B=\mu_0(H+M),

where μ0\mu_0 is the vacuum permeability. Hysteresis is commonly displayed as either an MM–HH loop or a BB–HH loop. These contain related information but have different intercepts and different behavior at high fields.

Starting from a demagnetized state, an increasing field usually produces an initial magnetization curve. At sufficiently high fields, the magnetization approaches saturation, meaning that most magnetic moments are aligned with the field. The saturation magnetization is denoted MsM_s. Even after MM is nearly saturated, BB continues to increase because of the μ0H\mu_0H contribution.

Reducing the field to zero generally leaves a nonzero magnetization. Applying a reverse field can then bring the magnetization through zero and toward saturation in the opposite direction. Completing the field cycle traces the other branch of the loop.

Remanence and coercivity

Two central measures characterize a hysteresis loop:

  • Remanence is the magnetization or flux density remaining after the applied field is removed, under a specified magnetic history. Saturation remanence is measured after prior saturation.
  • Coercivity is the magnitude of the reverse field required to reduce a specified magnetic quantity to zero after magnetization.

The distinction between the two common coercivities is important. The normal coercivity, HcBH_{cB}, is determined where B=0B=0; the intrinsic coercivity, HcJH_{cJ}, is determined where the magnetic polarization J=μ0MJ=\mu_0M, and therefore MM, is zero. These can differ substantially in permanent-magnet materials.

A major loop is obtained by cycling between fields sufficient to approach positive and negative saturation. Reversals made before saturation produce minor loops, whose shapes depend on the previous turning points. Some materials exhibit return-point memory: under appropriate conditions, returning to an earlier reversal field restores an earlier magnetic state. This is not a universal property of all magnetic systems.

Microscopic origin

In many bulk ferromagnets, magnetization is organized into magnetic domains: regions within which magnetic moments are approximately aligned. A specimen can have little net magnetization even when each domain is strongly magnetized, because differently oriented domains partially cancel one another.

An applied field changes the magnetic structure through several processes:

  • Motion of the boundaries, or domain walls, between domains.
  • Rotation of magnetization within domains.
  • Nucleation and growth of regions with a new magnetization direction.
  • Collective or nonuniform reversal of magnetic moments.

These processes are governed by competing energy contributions. Exchange interactions favor alignment of nearby moments; magnetic anisotropy favors particular magnetization directions; magnetostatic interactions depend on the specimen’s magnetic configuration and shape; and elastic stresses can influence magnetization through magnetoelastic coupling.

Defects, grain boundaries, inclusions, and internal stress can impede domain-wall motion. A wall may remain trapped until the field becomes strong enough to overcome a local energy barrier. Once released, it can jump abruptly to another configuration. Such discontinuous changes produce the Barkhausen effect.

Hysteresis therefore reflects irreversible transitions among metastable magnetic states. It is not simply a delay caused by a rapidly changing field: a substantial loop can remain even when the field is varied very slowly.

Domain-wall motion is not the only mechanism. A sufficiently small single-domain particle may reverse primarily by rotation or other nonuniform processes without containing a stable domain wall. Magnetic history dependence can also arise from flux pinning in materials exhibiting superconductivity, through a mechanism distinct from ferromagnetic domain reversal.

Energy loss

A closed hysteresis loop represents irreversible magnetic work during a cycle. For a uniformly magnetized specimen under a collinear cyclic field, the energy dissipated per unit volume is given by the loop area:

wloss=∮H dB.w_{\mathrm{loss}}=\oint H\,\mathrm{d}B.

For a closed cycle, the relation between BB, HH, and MM gives

wloss=μ0∮H dM.w_{\mathrm{loss}} =\mu_0\oint H\,\mathrm{d}M.

With the physical traversal direction, these expressions give a positive loss; geometrically, the relevant quantity is the enclosed area. A BB–HH loop area has units of joules per cubic metre. An MM–HH loop area must be multiplied by μ0\mu_0 to obtain the same units.

Much of this energy ultimately becomes heat. Under fixed cycling conditions, the corresponding average power loss per unit volume is

physt=f wloss,p_{\mathrm{hyst}}=f\,w_{\mathrm{loss}},

where ff is the cycle frequency. This proportionality does not imply that the loop area is independent of frequency.

In an alternating-current magnetic core, measured losses can also include eddy-current heating and additional dynamic contributions associated with magnetization reversal. A loop measured at finite frequency may therefore enclose more area than the quasistatic hysteresis loop. Laminated cores and electrically resistive magnetic materials reduce eddy-current losses, but do not automatically eliminate intrinsic hysteresis.

Soft and hard magnetic materials

The terms soft and hard describe magnetic reversal behavior, not necessarily mechanical hardness.

Soft magnetic materials have relatively low coercivity and are readily magnetized and demagnetized. Their narrow loops make them useful in transformer cores, inductors, electrical machines, and magnetic shielding. Examples include suitable grades of electrical steel, soft ferrites, and amorphous or nanocrystalline magnetic alloys. Performance depends on permeability, saturation magnetization, operating frequency, temperature, and losses, not coercivity alone.

Hard magnetic materials resist reversal and generally have larger coercivity. They are used in permanent magnets and magnetic recording. Examples include hard ferrites, samarium–cobalt magnets, and neodymium–iron–boron magnets. Useful permanent-magnet performance also requires adequate remanence and resistance to demagnetization under operating conditions.

For permanent magnets, an important specification is the maximum energy product, (BH)max⁡(BH)_{\max}, obtained from the second quadrant of the demagnetization curve. It characterizes the magnet’s ability to support a magnetic field in an external magnetic circuit and is distinct from the energy dissipated around a full hysteresis loop.

Temperature, time, and specimen geometry

Hysteresis is not a single immutable property of a chemical composition. It depends on microstructure, preparation, measurement conditions, and sample geometry.

Temperature and magnetic relaxation

Increasing temperature changes magnetic ordering, anisotropy, and the rate of thermally activated reversal. Above its Curie temperature, an ordinary ferromagnet loses spontaneous ferromagnetic order.

In sufficiently small magnetic particles, thermal fluctuations can reverse the particle’s magnetization over the observation period. In the superparamagnetic regime, a particle ensemble may show negligible remanence and coercivity on that timescale, even though individual particles retain internally ordered moments. The associated blocking temperature therefore depends on the measurement timescale.

Below such a regime, magnetization can still evolve slowly at fixed field through thermally activated transitions. This time dependence is often called magnetic viscosity or magnetic relaxation.

Demagnetizing fields

The field inside a magnetized specimen generally differs from the externally applied field because the specimen produces its own demagnetizing field. For a uniformly magnetized ellipsoid along a principal axis,

Hint=Happl−NM,H_{\mathrm{int}}=H_{\mathrm{appl}}-NM,

where NN is the dimensionless demagnetizing factor in the SI convention.

Consequently, loops plotted against applied field can depend strongly on specimen shape. Comparing intrinsic material properties requires attention to internal-field corrections, magnetic circuit geometry, and the possibility of nonuniform magnetization.

Measurement and modeling

Hysteresis loops are measured using induction-based instruments, vibrating-sample magnetometers, superconducting quantum interference device magnetometers, and other magnetometric methods. Inductive measurements obtain changes in magnetic flux through Faraday’s law of induction, while other instruments determine magnetic moment more directly.

Meaningful comparisons require specification of:

  • Maximum applied field and whether saturation was reached.
  • Field orientation and specimen geometry.
  • Temperature and field sweep rate or frequency.
  • Initial magnetic state and cycling history.
  • Background subtraction and calibration procedures.

Several models describe different aspects of hysteresis. The Preisach model represents a material as a distribution of elementary switching units and is useful for history-dependent behavior and minor loops. The Jiles–Atherton model represents reversible and irreversible magnetization changes through phenomenological equations. Micromagnetic models resolve spatially varying magnetization using exchange, anisotropy, magnetostatic, and applied-field energies.

These approaches are not interchangeable. Agreement with a major loop does not guarantee accurate minor loops, dynamic losses, or behavior under rotating fields. Parameters inferred from a fit need not uniquely identify microscopic mechanisms.

Historical development and applications

James Alfred Ewing established the term hysteresis in magnetic research during the 1880s. Charles Proteus Steinmetz later developed an influential empirical relation between magnetic hysteresis loss and the peak flux density, helping engineers estimate losses in alternating-current equipment. Such empirical loss relations remain useful within calibrated ranges, but their coefficients and validity depend on material, waveform, temperature, and frequency.

Magnetic hysteresis has several major practical roles:

  • Permanent magnets: stable remanence provides magnetic fields without continuous electrical excitation.
  • Magnetic recording and memory: distinguishable magnetization states retain information after the writing field is removed.
  • Power equipment: hysteresis loss contributes to heating and reduced efficiency in transformers, motors, generators, and inductors.
  • Magnetic characterization: loop shape and reversal behavior reveal changes in microstructure, stress, anisotropy, and magnetic interactions.
  • Demagnetization: an alternating field of gradually decreasing amplitude can reduce the net remanence of a suitable specimen, although it does not remove its local magnetic ordering.